Polymer Property : Flash Point = 246 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 119 °C
246 °F
closed cup
Dow Corning Z-6228 SILANE
Dow Corning® Z-6228 Silane is a dialkyldimethoxysilane. Silanes and siloxanes have been used for some time in this application to increase yield and improve the stereoregularity of the polyolefin r..
Flash Point 119 °C
246 °F
Method A; ASTM D93
ExxonMobil Exxsol™ D120 Dearomatized Fluid
Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil