Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | -4.40 °C | 24.1 °F | |
Permabond QFS10 Cyanoacrylate Activator The PERMABOND QFS 10 accelerates the cure of cyanoacrylate adhesives to provide a shorter set time. It can be used in a variety of applications but is especially useful when bonding porous or poorly.. |