Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 114 °C | 237 °F | Method A; ASTM D93 |
ExxonMobil Exxsol™ D110 Dearomatized Fluid Availability: Asia Pacific, Central America, North America and South AmericaAppearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Flash Point | 114 °C | 237 °F | |
BASF Vinyl Caprolactam Formula: C8H13NOCAS: 2235-00-9Description: Vinyl caprolactam is a yellowish solid, with a faint specific odor. It is soluble in water.Synonyms: NVC, Vinyl-caprolactameApplications: Intermediate use.. |
|||
Flash Point | 114 °C | 237 °F | |
BASF 2-Ethylhexanoic Acid Formula: C8H16O2CAS: 149-57-5Description: 2-Ethylhexanoic acid is a colorless to yellow liquid, with a faint specific odor. It is immiscible with water, but miscible with almost all conventional or.. |