Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 23.0 °C | 73.4 °F | |
Oceanchem Group Bromobutane (N-Butyl Bromide) Molecular Formula: C4H9BrCas No.: 109-65-9Application: Organic SynthesisStorage: The product should be stored in a cool and dry place.Information Provided by Oceanchem Group |
|||
Flash Point | 23.0 °C | 73.4 °F | Seta |
Lord Adhesives Flocklok® P11 Adhesive Flocklok® P11 is a moisture curing, flexible polyurethane adhesive used for automotive weatherstrip sealing profiles to flock. This adhesive will adhere polyester or polyamide flock to a variety .. |
|||
Flash Point | 23.0 °C | 73.4 °F | Seta |
Lord Adhesives Flocklok® P13 Adhesive Flocklok® P13 is a moisture curing, flexible polyurethane adhesive used for automotive weatherstrip sealing profiles to flock. This adhesive will adhere polyester or polyamide flock to a variety .. |
|||
Flash Point | 23.0 °C | 73.4 °F | ASTM D3278, Seta Flash, Closed Cup |
Lord Adhesives Chemglaze® V300 Polyurethane Coating Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m.. |