Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 96.0 °C | 205 °F | closed cup |
Dow Corning Z-6011 SILANE Dow Corning® Z-6011 Silane is a reactive chemical containing an aminopropyl organic group and a triethoxysilyl inorganic group. Chemically, Dow Corning® Z-6011 Silane is designated gammaaminopropy.. |
|||
Flash Point | 96.0 °C | 205 °F | |
ChevronTexaco 5606G Aircraft Hydraulic Oil Texaco Aircraft Hydraulic Oil 5606G delivers value through:Minimum viscosity change over a range of operating temperaturesLow pour point which permits operation at the lowest temperatures generally .. |
|||
Flash Point | 96.1 °C | 205 °F | Method A; ASTM D93 |
ExxonMobil Exxsol™ D95 Dearomatized Fluid Availability: Asia Pacific, Central America, North America and South AmericaAppearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Flash Point | 96.0 °C | 205 °F | ASTM D92 |
ChevronTexaco Aviation G Hydraulic Fluid FeaturesChevron Aviation Hydraulic Fluids are both manufactured from specially selected, highly refined, low viscosity and low pour point petroleum base stocks. They both contain a superior, shear .. |
|||
Flash Point | 96.0 °C | 205 °F | |
BASF Butane-2,3-diol Formula: C4H10N2CAS: 513-85-9Description: 2,3-Butandiol is a colorless to yellowish liquid, and is odorless. It is partly miscible with water.Synonyms: 2,3-ButandiolApplications: Intermediate used .. |
|||
Flash Point | 96.0 °C | 205 °F | |
BASF Dibutylethanolamin Formula: C10H23NOCAS:102-81-8Description: Dibutylethanolamine is a colorless to yellow liquid with an amine-like odor.Synonyms: DBEA, 2-Dibutylaminoethanol, Dibutylethanolamine, N,N-Dibutylethanolam.. |