Polymer Property : Flash Point = 191 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 88.5 °C
191 °F
Closed cup
Dow Corning BY 25-337 Silicone Emulsifier
This emulsifier for water-in-oil and water-in-silicone emulsions can be used in a wide range of personal care applications such as skin care, color cosmetics, sun care, hair care, and antiperspirant..