Flash Point 183 °C
361 °F
ASTM D92
ChevronTexaco Shingle Oil
FeaturesChevron Shingle Oil is a straw colored, low viscosity oil designed for use as a shingle or shake dressing for shake roofs, wooden fencing, wood siding, and log homes.Chevron Shingle Oil pene..