Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 81.7 °C | 179 °F | ASTM D92 |
ChevronTexaco ParaLux® 701R Process Oil FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with sup.. |