Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 173 °C | 343 °F | ASTM D92 |
ChevronTexaco ISO 15 Handy Oil FeaturesChevron Handy Oil is a highly refined, light-bodied, multipurpose lubricating oil.It contains an oxidation inhibitor to improve its natural stability and prevent the formation of gums and va.. |
|||
Flash Point | 173 °C | 343 °F | |
BASF Dimethyldicykan 3,3’-Dimethyl-4,4’-diamino-dicyclohexylmethane Formula: C15H30N2CAS: 6864-37-5Description: Dimethyldicykan is a colorless to yellow liquid with an amine-like odor.Synonyms: Dimethylidicykan, DMDC, Bis(3-methyl-4-aminocyclohexyl)methane, 4,4’-Me.. |