Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 172 °C | 342 °F | ASTM D92 |
ExxonMobil Thermrex Series R-21 The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and .. |
|||
Flash Point | 172 °C | 342 °F | See Note 3. |
ChevronTexaco 904 Grease NLGI Grade 1/2 Texaco 904 Grease is a calcium soap grease. It contains graphite which enhances its lubricity.Typical test data are average values only. Minor variations which do not affect product performance are .. |
|||
Flash Point | 172 °C | 342 °F | ASTM D92 |
ExxonMobil Thermrex Series R-21 The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and .. |