Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 164 °C | 327 °F | |
BASF N4-Amine N,N’-Bis-(3-Aminopropyl)ethylene-diamine Formula: C8H22N4CAS: 10563-26-5Description: N4 Amine is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: 4,7-Diazadecane-1,10-diamine, 1,5,8,12-Tetraazadodeca.. |
|||
Flash Point | 164 °C | 327 °F | |
BASF N4-Amine S N,N'-Bis-(3-Aminopropyl)ethylene-diamine Formula: C8H22N4CAS: 10563-26-5Description: N4-Amine S is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: 1,3-Propanediamine,N,N”-1,2-ethanediylbis- 1,5,8,1.. |