Polymer Property : Flash Point = 16.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 16.0 °C
60.8 °F
Lord Adhesives 403 Flexible, High Impact and Peel Resistance, Fast Cure Acrylic Adhesive
Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e..
Flash Point 16.0 °C
60.8 °F
Lord Adhesives 410 Flexible, High Impact and Peel Resistance, Long Working Time Acrylic Adhesive
Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e..
Flash Point 16.0 °C
60.8 °F
Seta
Lord Adhesives Flocklok® 870 Flock Adhesive
LORD Flocklok® 870 adhesive is a single-coat adhesive used to adhere polyester or nylon flock if beers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good r..
Flash Point 16.0 °C
60.8 °F
closed cup
Dow Corning Z-6026 SILANE
Dow Corning® Z-6026 Silane is a chemically reactive material composed of an amino-alkyltrimethoxysilane and a polyol diluted to 40% by weight in methanol. Chemically, it is similar to Dow Corning®..
Flash Point 16.0 °C
60.8 °F
COC
3M Scotch-Weld™ 3901 Metal Primer
3M™ Scotch-Weld™ Metal Primer 3901 is a primer for 3M™ Scotch-Weld™ film and liquid adhesives in those applications where it is desired to obtain improved metal and glass adhesion or improved re..