Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 158 °C | 316 °F | ASTM D92 |
ExxonMobil 422 Mobilmet 400 Series Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation.. |
|||
Flash Point | 158 °C | 316 °F | ASTM D92 |
ExxonMobil 422 Mobilmet 400 Series Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation.. |
|||
Flash Point | 158 °C | 316 °F | |
ChevronTexaco Alcaid® 13 Texaco Alcaid® oils deliver value through:Low pour points that permit oils to remain fluid at subzero temperatures.Ready separation from water, an important property where severe moisture condition.. |