Polymer Property : Flash Point = 152 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point >= 152 °C
>= 306 °F
uncork
Hong Kun Group AO 1135 Antioxidant
This product is phenols antioxidant, applicable to the occasion that there are liquor, latex, soliquoid and mixture,especially applicable to polyols and polyurethane.it has excellent effect in anti-..
Flash Point >= 152 °C
>= 306 °F
DIN 51758
BASF Caprolactam Liquid
Recommended use: Initial product for chemical syntheses, for the production of homopolymerisates and copolymerisatesInformation provided by BASF
Flash Point >= 152 °C
>= 306 °F
DIN 51758
BASF Caprolactam Tablets
Recommended use: For the production of homopolymerisates and copolymerisates, initial product for chemical synthesesInformation provided by BASF
Flash Point 152 °C
306 °F
BASF 2-Butyne-1,4-diol Pure Cryst.
Formula: C6H15NOCAS: 110-65-6Description: N-Butyldiethanolamine is a colorless to yellow liquid with an amine-like odor. It is miscible with water in all proportionsSynonyms: BDEA, N-Butyldiethanol..