Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 144 - 146 °C | 291 - 295 °F | Closed Cup |
Solvay RHODISOLV® PORLARCLEAN Solvent Description: Rhodiasolv PolarClean is a eco-friendly water soluble polar solvent or co-solvent very effective to solubilize agrochemicals. It is recommended to use in EC’s (emulsifiable concent.. |