Polymer Property : Flash Point = 118 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 118 °C
244 °F
ASTM D93
ExxonMobil Vacmul 3 D
Vacmul 3 D is a non-staining, medium-duty, mineral oil-based honing and grinding fluid. It is designed for operation where more difficult-to-machine metals are used. It performs well on both ferrous..
Flash Point 118 °C
244 °F
ASTM D93
ExxonMobil Vacmul 3 D
Vacmul 3 D is a non-staining, medium-duty, mineral oil-based honing and grinding fluid. It is designed for operation where more difficult-to-machine metals are used. It performs well on both ferrous..
Flash Point 118 °C
244 °F
ASTM D56
ExxonMobil Varsol™ 110 Non-dearomatized Fluid
Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation provided by ExxonMobil
Flash Point 118 °C
244 °F
BASF N-Formylmorphonline
Formula: C5H9NO2CAS: 4394-85-8Description: N-Formylmorpholine is a colorless to yellowish solid or liquid that is odorless.Synonyms: 4-Morpholinecarbaldehyde, Formylmorpholine, NFMApplications: Inte..