Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 102 °C | 215 °F | ASTM D56 |
Humiseal 1C49 Silicone Conformal Coating Humiseal 1C49 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-4605.. |
|||
Flash Point | 102 °C | 216 °F | ASTM D92 |
ExxonMobil Mobil Velocite 4 The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra.. |
|||
Flash Point | 102 °C | 216 °F | open cup |
Dow Corning Z-6062 SILANE Dow Corning® Z-6062 Silane is an organofunctional reactive silane. It has a mercaptopropyl and organic group.Information provided by Dow Corning |
|||
Flash Point | 102 °C | 216 °F | ASTM D92 |
ExxonMobil Mobil Velocite 4 The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra.. |
|||
Flash Point | 102 °C | 216 °F | ASTM D92 |
ChevronTexaco Aviation A Hydraulic Fluid FeaturesChevron Aviation Hydraulic Fluids are both manufactured from specially selected, highly refined, low viscosity and low pour point petroleum base stocks. They both contain a superior, shear .. |