Polymer Property : Flash Point = 100 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point -4.00 - 100 °C
24.8 - 212 °F
Average value: 33.0 °C Grade Count:4
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..