Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 1.60 °C | 34.9 °F | Seta |
Lord Adhesives Chemlok® AP-134 One-Coat Primer Chemlok® AP-134 is a clear, low viscosity, solventborne reactive primer which can function as a primer or adhesive for a variety of polar substrates. Substrates include: steel, aluminum, brass, E.. |