Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | -45.0 °C | -49.0 °F | |
BASF Ethylvinylether Stabilized 0.01% KOH Formula: C4H8OCAS: 109-92-2Description: Ethylvinylether is a colorless liquid with an ether-like odor.Synonyms: Ethoxyethen, Vinylethylether, VEE, 1-Ethoxyethylene, Ethoxy-ethen, EVE, Ethyl Vinyl Et.. |
|||
Flash Point | -45.0 °C | -49.0 °F | |
BASF Ethylvinylether Stabilized 0.1% KOH Formula: C4H8OCAS: 109-92-2Description: Ethylvinylether is a colorless liquid with an ether-like odor.Synonyms: Ethoxyethen, Vinylethylether, VEE, 1-Ethoxyethylene, Ethoxy-ethen, EVE, Ethyl Vinyl Et.. |
|||
Flash Point | -45.0 °C | -49.0 °F | |
BASF Ethylvinylether Stabilized 0.01% DEA Formula: C4H8OCAS: 109-92-2Description: Ethylvinylether is a colorless liquid with an ether-like odor.Synonyms: Ethoxyethen, Vinylethylether, VEE, 1-Ethoxyethylene, Ethoxy-ethen, EVE, Ethyl Vinyl Et.. |