Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | -17.8 °C | -0.0400 °F | |
BASF N-Methylpyrrolidine Formula: C5H11NCAS: 120-94-5Description: N-Methylpyrrolidine is a colorless to yellowish liquid with an amine-like odor. It is miscible in water.Synonyms: 1-Methylpyrrolidin, N-Methyltetrahydropyrr.. |