Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flash Point = -1.00 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point -1.00 °C
30.2 °F
Closed Cup
Dow Corning XIAMETER® PMCPPMX-200, 0.65CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID .65CS. A volatile siloxane fluid (hexamethyldisiloxane).Information provided by Dow Corning