Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | -0.500 °C | 31.1 °F | Pensky-Martin Closed Cup |
Momentive Performance Materials SS4120 Silicone Primer for use with RTV Silicone Adhesive Sealants, Clear SS4004P, SS4044P, SS4120, SS4155, and SS4179 primers are formulated for use with GE Silicones RTV silicone rubber adhesive sealants. GE Silicones one-component products offer primerless adhesion.. |