Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 5500 °C | 9930 °F | |
Reade Advanced Materials Calcia Stabilized Zirconium Oxide (ZrO2 + CaO) Description: Produced by thermal processes. Used in wear parts, engine and machine components, mill media, refractories, ceramic pigments. fuel cells, laser, and capacitors.Forms Available: Various.. |