Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 94.0 °C | 201 °F | |
BASF N-Butyl Vinyl Ether Formula: C6H12OCAS: 11-34-2Description: N-Butyl vinyl ether is a colorless to yellow liquid, with an ether-like odor. It is sparingly soluble in water.Synonyms: NBVE, 1-(Vinyloxy)butane, 1-(Ethenyl.. |