Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | >= 31.0 °C | >= 87.8 °F | Initial |
Kazanorgsintez E-16 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Boiling Point | 31.0 - 33.0 °C | 87.8 - 91.4 °F | |
BASF Isopropylamine Formula: C3H9NCAS: 75-31-0Description: Isopropanolamine is a colorless to yellowish liquid with an amine-like odor. It is miscible in water.Synonyms: 1-Amino-2-propanol, Monoisopropanolamin, 1-Amin.. |