Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | >= 30.0 °C | >= 86.0 °F | Initial |
Kazanorgsintez E-11 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Boiling Point | >= 30.0 °C | >= 86.0 °F | Initial |
Kazanorgsintez E-15 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |