Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 78.0 °C | 172 °F | at 760 mmHg |
LyondellBasell Ethanol, 200 Proof Information provided by Lyondell. |
|||
Boiling Point | 78.0 - 82.0 °C | 172 - 180 °F | |
BASF N-Methylpyrrolidine Formula: C5H11NCAS: 120-94-5Description: N-Methylpyrrolidine is a colorless to yellowish liquid with an amine-like odor. It is miscible in water.Synonyms: 1-Methylpyrrolidin, N-Methyltetrahydropyrr.. |
|||
Boiling Point | 78.0 °C | 172 °F | of Solvent |
3M Novec™ 2704 Electronic Grade Coating 3M™ Novec™ 2704 Electronic Grade Coating is designed for the protection of printed circuit boards and electronic components. It is a clear, low viscosity solution of a 4 wt% fluoropolymer carried .. |