Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 240 - 370 °C | 464 - 698 °F | |
BASF AMIX TI Formula: C9H21NO3CAS: 122-20-3Description: AMIX TI is a dark solid that is almost odorless. It is fully soluble in waterSynonyms: TRIPA, 1,1’,1”-Nitrilotri-2-propanol, Tri-2-propanolamine, Tri-is.. |