Boiling Point 347 °C
657 °F
BASF Dimethyldicykan 3,3’-Dimethyl-4,4’-diamino-dicyclohexylmethane
Formula: C15H30N2CAS: 6864-37-5Description: Dimethyldicykan is a colorless to yellow liquid with an amine-like odor.Synonyms: Dimethylidicykan, DMDC, Bis(3-methyl-4-aminocyclohexyl)methane, 4,4’-Me..