Thermal Properties Metric English Comments
Boiling Point 54.0 °C
129 °F
Asahi Glass ASAHIKLIN AK-225 Hydrochlorofluorocarbon Solvent
Asahilkin AK-225 is an environmentally sensible hydrochlorofluorocarbon (HCFC) designed to replace chlorofluorocarbon (CFC), perfluorocarbon (PFC), and other HCFCs with high ODP values in a variety ..
Boiling Point 54.0 °C
129 °F
Asahi Glass ASAHIKLIN AK-225DH Hydrochlorofluorocarbon Solvent
AK-225DH was developed as a solvent dewatering and drying system to remove water from the surface of various parts and assemblies. AK-225DH is a mixture of AK-225 and a drying agent to give it rapid..
Boiling Point 54.0 °C
129 °F
Asahi Glass ASAHIKLIN AK-225T Hydrochlorofluorocarbon Solvent
AK-225T is a mixture of AK-225, ethanol, hydrocarbon and stabilizers. This blend was developed for those customers needing a more aggressive defluxer than AK_225AES. It has proven to be effective in..