Thermal Properties Metric English Comments
Boiling Point 275 - 287 °C
527 - 549 °F
LG Chemical TOTM Plasticizer
Features: LG TOTM is used in cable and sheet by product that aging property and migration resistance among our products are superior.Application: Power cableInformation provided by LG Chemical
Boiling Point 275 °C
527 °F
Initial; ASTM 1078
ExxonMobil Exxsol™ D140 Dearomatized Fluid
Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil