Thermal Properties Metric English Comments
Boiling Point 270.8 °C

@Pressure 0.1031 MPa
519.4 °F

@Pressure 14.96 psi
BASF Caprolactam Liquid
Recommended use: Initial product for chemical syntheses, for the production of homopolymerisates and copolymerisatesInformation provided by BASF
Boiling Point 270.8 °C

@Pressure 0.1031 MPa
519.4 °F

@Pressure 14.96 psi
BASF Caprolactam Tablets
Recommended use: For the production of homopolymerisates and copolymerisates, initial product for chemical synthesesInformation provided by BASF