Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 261 °C | 502 °F | |
BASF Lupragen® N 700 1,8-Diazabicyclo-5,4,0-undecene-7 Formula: C7H18N2OCAS: 6674-22-2Description: Lupragen® N 700 –1,8-Diazabicyclo-5,4,0-undecene-7 is a colorless to yellowish liquid, with an amine-like odor. It is miscible with water in all propor.. |