Polymer Property : Boiling Point = 495 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 257 °C
495 °F
Initial; ASTM D86
ExxonMobil Varsol™ 120 Non-dearomatized Fluid
Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and EuropeInformation provided by ExxonMobil