Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 255 °C | 491 °F | Initial; ASTM 1078 |
ExxonMobil Exxsol™ D120 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Boiling Point | 255 - 256 °C | 491 - 493 °F | |
BASF Imidazole Formula: C3H4N2CAS: 288-32-4Description: Imidazole is a crystalline powder with an amine-like odor. It is soluble in water.Synonyms: 1,3-Diaza-2,4-cyclopentadiene, 1,3-Diazole, Imidazol, Methanimid.. |