Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 234 °C
453 °F
Initial; ASTM 1078
ExxonMobil Exxsol™ D100 Dearomatized Fluid
Availability: Africa & Middle East, Europe and South America Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil
Boiling Point 234 °C
453 °F
Final; ASTM 1078
ExxonMobil Exxsol™ D220/230 Dearomatized Fluid
Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil