Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 178 °C | 352 °F | Initial; ASTM D86 |
ExxonMobil Isopar™ H (EU) Isoparaffin Fluid Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and Eu.. |