Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 315 °C | 599 °F | Final; ASTM 1078 |
ExxonMobil Exxsol™ D140 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |