Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Boiling Point = 309 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 309 °C
588 °F
BASF Lupragen® 106 2,2'-Dimorphalinyldiethylether
Formula: C12H24N2O3CAS: 6425-39-4Description: 2,2’-Dimorpholinyldiethylether is a colorless to yellow liquid, with an amine-like odor. It is also miscible with water.Synonyms: DMDEE, Morpholone 4,..