Thermal Properties Metric English Comments
Boiling Point 298 °C
568 °F
Final; ASTM 1078
ExxonMobil Exxsol™ D120 Dearomatized Fluid
Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil
Boiling Point 298 °C
568 °F
BASF DODA 4,9-Dioxadodecane,1-12-diamine
Formula: C