Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 279 °C | 534 °F | Initial; ASTM D86 |
ExxonMobil Exxsol™ D130 Dearomatized Fluid Availability: Asia Pacific, Central America, North America and South AmericaAppearance: Clear/Transparent LiquidInformation provided by ExxonMobil |