Polymer Property : Boiling Point = 270 °F
Polymer Property :
Boiling Point =
270 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Boiling Point
132
°C
270
°F
at 760 mmHg
LyondellBasell PE Propylene glycol ethyl ether
Information provided by Lyondell.