Polymer Property : Boiling Point = 2519 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 2519 °C
4566 °F
American Elements Aluminum Nanoparticles
General DescriptionAluminum (Al) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Aluminum Particles are typically 10-30 nanometers (nm) with sp..