Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 219 °C | 426 °F | Initial; ASTM 1078 |
ExxonMobil Exxsol™ D220/230 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |