Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Boiling Point = 205 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 96.0 - 97.0 °C
205 - 207 °F
BASF Epsilon-Caprolactone
Formula: C6H10O2CAS: 502-44-3Description: Epsilon-caprolactone is a colorless to yellow liquid, with a perceptible odor. It is soluble in water.Synonyms: 6-Hydroxyhexanoic acid lactone, Caprolacton..