Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 90.0 °C | 194 °F | |
Solvay Specialty Polymers PERFLUOROSOLVâ„¢ PFS1 Perfluorinated Cleaning Solvent PERFLUOROSOLV PFS-1 is a low molecular weight perfluoropolyether solvent and diluent that perfroms well in many electronic and semiconductor cleaning functions, such as: pump cleaning, degreasing, d.. |
|||
Boiling Point | 90.0 °C | 194 °F | |
BASF Triethylamine TEA Formula: C6H15NCAS: 121-44-8Description TEA is a colorless liquid. It is miscible with nearly every common organic solvent.Synonyms: TEA, N,N-Diethylethanamine, (Diethylamino)ethaneApplications: In.. |
|||
Boiling Point | 90.0 - 100 °C | 194 - 212 °F | |
BASF ptBCF 4-tert.-Butylcyclohexyl choroformate Formula: C11H19ClOCAS: 42125-46-2Description: ptBCF is a colorless to yellow liquid with a pungent odor.Synonyms: 4-t-Butylcyclohexyl chlormiat, Carbonochloride acid, 4(1,1-dimethylethyl)cyclohexyle.. |
|||
Boiling Point | 90.0 - 92.0 °C | 194 - 198 °F | |
BASF N-Vinyl-2-pyrrolidone, Non-Stabilized Formula: C6H9NOCAS: 88-12-0Description: Vinyl pyrrolidone is a colorless to yellowish liquid, with a characteristic odor. It is miscible in water and organic solvents.Synonyms: N-Vinylpyrrolidone, .. |