Thermal Properties Metric English Comments
Boiling Point 81.0 °C
178 °F
Solvay Specialty Polymers Galden® DET PFPE Fluid
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat..