Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 158 °C | 316 °F | Initial; ASTM D86 |
ExxonMobil Varsol™ 1 Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: Central America, North America and South AmericaInformation provided by ExxonMobil |
|||
Boiling Point | 158 °C | 316 °F | Initial; ASTM D86 |
ExxonMobil Varsol™ 40 Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and EuropeInformation provided by ExxonMobil |
|||
Boiling Point | 158 - 159 °C | 316 - 318 °F | |
BASF Isopropanolamine Formula: C3H9NOCAS: 78-96-6Description: Isopropanolamine is a colorless to yellowish liquid with an amine-like odor. It is miscible in water.Synonyms: 1-Amino-2-propanol, Monoisopropanolamin, 1-Ami.. |