Thermal Properties Metric English Comments
Boiling Point 57.6 °C
136 °F
Dow Corning Z-1229 TETRACHLOROSILANE
Fiber optic gradeInformation provided by Dow Corning
Boiling Point 57.8 °C
136 °F
Initial; ASTM 1078
ExxonMobil Exxsol™ Isohexane Dearomatized Fluid
Availability: Africa & Middle East, Asia Pacific and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil
Boiling Point 57.7 °C
136 °F
Dow Corning Z-1224 TRIMETHYLCHLOROSILANE
Information provided by Dow Corning
Boiling Point 58.0 °C
136 °F
Asahi Glass ASAHIKLIN AK-225FPL Hydrochlorofluorocarbon Solvent
AK-225FPL is a mixture of HCFC-225 and a fluorinated solvent. This blend was developed for those customers needing a solvent which is compatible with common plastics, such as polymethylmethacrylate,..